Features: Excellent chemical resistance performance
Applicable environment: Chemical plant, chemical fertilizer plant, paper-making factory
Technical data:
Physical property of cover rubber under hot air accelerated aging test (test condition: 70℃*96h)
ITEM | Breaking strength,MPa | Elongation at break,% | abrasion,mm3 | hardness,(°) |
Performance before agingg | ≥14.0 | ≥400 | ≤250 | 60±5 |
Performance after aging | ≥12.0 | ≥340 | --- | 65±10 |
Note: When the thickness of the cover rubber is 0.8mm-1.6m, the sample thickness can be the maximum cut length, the tensile strength and the elongation at break are allowed to be 15% lower than those in the table. | |
--Product Display -----------------------------------------------------------------------------------------
--Production Process-----------------------------------------------------------------------------------------
--Factory Site --------------------------------------------------------------------------------------------------
--Certificate----------------------------------------------------------------------------------------------------